Characterization of Aluminum Oxide–Hydroxyapatite Ceramic Composites Sintered with Hydroxyapatite at Various Concentrations and Post-sinter Degradation By-products Analysis: An In Vitro Spectroscopic Study
Ajay, Ranganathan and Balu, Kandasamy and Yasmin-Fathima, Jailaudeen (2025) Characterization of Aluminum Oxide–Hydroxyapatite Ceramic Composites Sintered with Hydroxyapatite at Various Concentrations and Post-sinter Degradation By-products Analysis: An In Vitro Spectroscopic Study. World Journal of Dentistry, 16 (1). pp. 8-13. ISSN 0976-6006
3.pdf
Download (39MB)
Abstract
Aim: To characterize newly formulated aluminum oxide–hydroxyapatite (AHA) ceramic composites sintered with hydroxyapatite (HA) incorporated
at four different concentrations and to ascertain the absence of post-sinter degradation by-products in the ceramic composite.
Materials and methods: Control group A contains plain sintered aluminum oxide (Al2O3). Four experimental groups were formulated and sintered
by admixing HA with Al2O3 at 2.5 wt% (group B), 5.0 wt% (group C), 7.5 wt% (group D), and 10 wt% (group E) concentrations. Field emission
scanning electron microscopy (FESEM) combined with energy dispersive X-ray (EDX) spectroscopy were employed for surface topographical
and elemental composition analysis, respectively. To detect post-sinter degradation by-products, X-ray diffraction (XRD) spectroscopy of ground
specimens was performed.
Results: Hydroxyapatite hexagonal crystallites were absent in the control group and were observed in all the experimental groups. There
were significant differences in the EDX spectra between the control and the experimental groups. EDX spectra showed peaks of calcium (Ca),
phosphorus (P), and calcium aluminates (CA) in all the experimental groups, thereby ascertaining the presence of undecomposed HA. An
exclusive peak corresponding to krotite appeared only in groups D and E.
Conclusion: The newly formulated AHA ceramic composites sintered with incorporated HA in all four concentrations do not contain post-sinter
degradation by-products, and the HA was not decomposed when sintered with Al2O3.
Clinical significance: Neither with any prior surface treatment nor with the use of primers, this novel attempt would be beneficial in chemically
bonding alumina-based ceramics with 10-methacryloxydecyl dihydrogen phosphate (10-MDP)-containing resin cements, thereby increasing
the clinical serviceability of the prostheses.
Keywords: Aluminum oxide, Calcium aluminate, Ceramic composite, Chemical characterization, Hydroxyapatite.
| Item Type: | Article |
|---|---|
| Subjects: | No Subjects |
| Divisions: | Prosthodontics and Crown and Bridge |
| Depositing User: | Unnamed user with email techsupport@mosys.org |
| Date Deposited: | 27 Oct 2026 05:41 |
| Last Modified: | 27 Oct 2026 05:41 |
| URI: | https://ir.vdcw.ac.in/id/eprint/328 |