Comparative Evaluation of Flexural and Impact Strengths of Glass Fiber- and Titanium Dioxide Nanoparticle-Reinforced Polymethyl Methacrylate Denture Base Resin: An In Vitro Study

Ponjayanthi, V and Vishali, S and Subramanian, Suganya and Peter, Claudia and Mani, Jeevitha and Maheswaran, Thangadurai (2026) Comparative Evaluation of Flexural and Impact Strengths of Glass Fiber- and Titanium Dioxide Nanoparticle-Reinforced Polymethyl Methacrylate Denture Base Resin: An In Vitro Study. Cureus. ISSN 2168-8184

[thumbnail of flextural srength.pdf] Text
flextural srength.pdf

Download (12MB)

Abstract

Objective: This in vitro study aimed to evaluate the effects of glass fiber and titanium dioxide (TiO₂)
nanoparticle reinforcement on the flexural and impact strengths of polymethyl methacrylate (PMMA)
denture base resin.
Methods: Forty rectangular heat-activated acrylic denture base specimens with dimensions of 65 mm × 10
mm × 3.3 mm and 80 mm × 4 mm × 10 mm were fabricated to determine the flexural and impact strengths in
accordance with ISO#1567 with an estimated sample size of 10 per group, which was further divided into
five for flexural and five for impact strength. Group 1 (Control group) contains conventional heat-activated
acrylic denture base resin, Group 2 has 2% TiO2 nanoparticle-incorporated heat-cured acrylic denture base
resin, Group 3 comprises 2% glass fiber-incorporated heat-cured acrylic denture base resin, and Group 4
(Hybrid group) comprises 2% TiO2+2% glass fiber-incorporated heat-cured acrylic denture base resin. The
fabrication followed the compression molding technique and a long curing cycle, and the specimens were
tested for flexural and impact strengths.
Result: The hybrid reinforcement group (Group 4; 2% TiO₂ + 2% glass fiber) demonstrated the highest
flexural strength (100.32 ± 4.21 MPa), followed by the glass fiber-reinforced group (Group 3; 92.71 ± 3.93
MPa), the TiO₂-reinforced group (Group 2; 84.87 ± 3.78 MPa), and the conventional PMMA group (Group 1;
76.35 ± 2.61 MPa). Similarly, the highest impact strength was observed in Group 4 (5.13 ± 0.43 kJ/m²),
followed by Group 3 (4.90 ± 0.39 kJ/m²), Group 2 (3.87 ± 0.45 kJ/m²), and Group 1 (1.48 ± 0.26 kJ/m²).
Conclusion: Hybrid reinforcement with TiO2 and glass fiber exhibited better flexural and impact strengths
than conventional TiO2 and glass fiber-reinforced PMMA.

Item Type: Article
Subjects: No Subjects
Divisions: Prosthodontics and Crown and Bridge
Depositing User: Unnamed user with email techsupport@mosys.org
Date Deposited: 27 Oct 2026 05:33
Last Modified: 27 Oct 2026 05:33
URI: https://ir.vdcw.ac.in/id/eprint/326

Actions (login required)

View Item
View Item